By definition, all 4# lines break at 4# of pressure. The same goes for 6#, 8#, 10#, etc. So, there is no “strongest” 4/6/8/10 pound line. That’s the theory, anyway. In practice, lines almost always “overtest”. That is, they are stronger than what it says on the package. All else being equal, a thicker line is a stronger line